ISSN 0430-6252. Physicochemical Mechanics of Materials. 2023.
Volume 59, Issue 1
Characteristics of the quality of deposited details treatment
Keywords
treatment, dopped materials, quality, rougness, machine parts.
Cite as
Kolomiyets V. V., Antoshchenkov R. V., Luk’yanenko V. M., Ridnyi R. V., Kharchenko S. O., Fabrychnikova I. A., Bohdanovych S. A., and Svirhun O. A. Characteristics of the quality of deposited details treatment. Physicochemical Mechanics of Materials. 2023. 59(1), 30-36.
https://doi.org/10.15407/pcmm2023.01.030
Abstract
The quality characteristics of the finishing treatment of deposited materials with cutting wires made of hard alloy and super hard material (hexanite-R) are investigated. It has been established that during finishing turning of the deposited parts, the low roughness of the machined surface is achieved when machining with hexanite-R cutters. The roughness of the machined surface depends on the feed the optimum cutting speed, the shape of the tool tip and its wear. The depth of the surface hardening of the machined layer with cutters is greater when turning the weld materials of low hardness. When turning with hexanite-R cutters, compressive residual compression stresses are formed in the surface layer, which improve the performance characteristics of parts.
References
- I. V. Dunin-Barkovskyi, and A. N. Kartashova, Measurement and Analysis of Surface Roughness, Waviness and Non-circularity [in Russian], Mashinostroyeniye, Moscow (1978).
- V. V. Kolomiets, R. V. Antoshchenkov, R. V. Ridnyi, S. A. Bogdanovich, and I. A. Fabrichnikova, “Optimization of the process of machining of inhomogeneous built-up parts of tractors,” Mater. Sci., 55, No. 1, 52-62 (2019). https://doi.org/10.1007/s11003-019-00251-w
- Cutting materials with blade tools. Vol. 3 in: F. V. Novikov and A. V. Yakimova (Eds.) Physical and Mathematical Theory of Material Processing Processes and Mechanical Engineering Technology [in Russian], Odessa Nat. Techn. Univ., Odessa (1973).
- A. V. Podzei (Ed.), Technical Residual Stresses [in Russian], Mashinostroyeniye, Moscow (1973).
- B. M. Sverdlova, and M. Ya. Fuks, “Features of the formation of residual stresses in heterophase materials and their change during operation [in Russian],” Sverkhtverdye Materialy, Is. 12, 3-9 (1981).
- V. V. Kolomiyets, R. V. Ridnyi, T. S. Skoblo, and S. A. Klimenko, “Analysis of methods for improving the operation properties of parts restored by hardening,” Visnyk of Kharkiv Nat. Techn. Univ. of Agriculture, Is. 10, 18-23 (2002).
- I. A. Ordinartseva (Ed.), Toolmaker’s Handbook [in Russian], Mashinostroyeniye, Moscow (1987).
- A. P. Pilyankevich, The Practice of Electron Microscopy [in Russian], Mashgiz, Moscow (1961).
- V. V. Kolomiyets, and Ye. V. Krasilnikov, “Electron microscopic study of the wear microrelief of cutters made of hexanite-R and elbor-R [in Russian],” Almazy i Sverkhtverdye Materialy, No. 9, 6-7 (1977).
- S. A. Klimenko, S. An. Klimenko, A. S. Manokhin, and V. M. Beresnev, “Features of application of cutting tools made of polycrystal cubic boron nitride with protection coating [in Ukrainian],” Sverkhtverdye Materialy, No. 4, 88-100 (2017). https://doi.org/10.3103/S1063457617040098
- A. S. Manokhin, S. A. Klimenko, S. An. Klimenko, and V. M. Beresnev, “Perspective type of coatings for tools covered with polycrystal cubic boron nitride (CBN) [in Ukrainian],” Nadtverdi Materialy, No. 6, 78-88 (2018).
- O. I. Balyts’kyi, V. O. Kolesnikov, and M. R. Havrylyuk, “Influence of modification of 38KhN3MFA steel on the structural-phase state and cutting products under variable technological conditions,” Mater. Sci., 55, No. 6, 915-920 (2020). https://doi.org/10.1007/s11003-020-00387-0
- V. V. Kolomiyets, L. N. Tyshchenko, S. A. Klimenko, M. V. Yerenemko, and L. N. Pereverzeva, “Use of technological lubricoolant during treatment of deposited materials by cutting,” Visnyk of Kharkiv Nat. Techn. Univ. of Agriculture, Is. 68, 20-23 (2008).
- V. I. Sorbat, and V. V. Kolomiyets, “Influence of technological parameters on roughness under turning of the surface deposited by Np-12Kh18N9T wire,” In collected papers “Dynamics of Aircraft Constructions”, Kharkov (1985), pp. 128-133.